Fractography of Glasses and Ceramics VI

Om Fractography of Glasses and Ceramics VI

Fractography of Glasses and Ceramics VI contains 25 papers presented at The Sixth Conference on the Fractography of Glasses and Ceramics held June 5-8, 2011 in Jacksonville, Florida. Papers deal with a variety of ceramics (silicon nitride, alumina, nanocomposites, laminates, dental ceramics, ceria, and zirconia), and glasses.

Visa mer
  • Språk:
  • Engelska
  • ISBN:
  • 9781118273739
  • Format:
  • Inbunden
  • Sidor:
  • 324
  • Utgiven:
  • 26. juli 2012
  • Mått:
  • 165x241x20 mm.
  • Vikt:
  • 581 g.
  Fri leverans
Leveranstid: 2-4 veckor
Förväntad leverans: 9. oktober 2025

Beskrivning av Fractography of Glasses and Ceramics VI

Fractography of Glasses and Ceramics VI contains 25 papers presented at The Sixth Conference on the Fractography of Glasses and Ceramics held June 5-8, 2011 in Jacksonville, Florida. Papers deal with a variety of ceramics (silicon nitride, alumina, nanocomposites, laminates, dental ceramics, ceria, and zirconia), and glasses.

Användarnas betyg av Fractography of Glasses and Ceramics VI



Hitta liknande böcker
Boken Fractography of Glasses and Ceramics VI finns i följande kategorier:

Gör som tusentals andra bokälskare

Prenumerera på vårt nyhetsbrev för att få fantastiska erbjudanden och inspiration för din nästa läsning.